Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 200 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
392 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola G-Etronax EP S Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: Particularly good electrical and mechanical properties by continuous use, even at high temperatures. Very good chemical resistance. Engineering and insulation material in electrical mac..
Maximum Service Temperature, Inert 200 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
392 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets
Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation ..
Maximum Service Temperature, Inert 200 °C

@Thickness 3.00 mm,
Time 7.20e+7 sec
392 °F

@Thickness 0.118 in,
Time 20000 hour
IEC 60695-11-10; IEC/EN 61212-2 7.1
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Tubes
Description: Extremely good mechanical properties, at high temperatures. Low thermal conductivity.Applications: Material for components used in the aerospace industry. Insulation parts in wire weldi..