Polymer Property : Maximum Service Temperature, Air = 123 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 113 - 123 °C
235 - 253 °F
Softening Range
Huntsman Araldite GT 7097 US Bisphenol A Epoxy Solid Resin
Weight per Epoxide (EEW, g/eq) 1500 to 2000. Max color is 3.Comments/Applications: Unmodified bis A "Type 7" epoxy. High melt viscosity epoxy for flow control in powder coatings and container coat..