Polymer Property : Maximum Service Temperature, Air = 1260 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 680 °C
1260 °F
100 to 10,000 hr, depends on temperature gradient
Schott ROBAX® Glass Ceramic
ROBAX® is a highly transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in flat, rolled s..