Thermal Properties Metric English Comments
Maximum Service Temperature, Air 730.0 °C
1346 °F
Intermittent
American Utility Metals Cromgard® Stainless Steel
Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o..