Thermal Properties Metric English Comments
Maximum Service Temperature, Air 139 - 143 °C
282 - 289 °F
Softening Range
Huntsman HT 2844 Special Hardener
Mix Ratio with 100 phr GT 7013 is 5.Comments/Applications: 0-toluyl giguanide. Dicy-type solid hardener for high gloss. *Mix ratio with GT 7013. Decorative and protective powder coatings.Data pr..