Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1500 °C | 2730 °F | no load |
McDanel Advanced Ceramics MV-HR1 Mullite Mullite (3Al2O3 • 2SiO2) is a refractory oxide material combining low thermal expansion, good mechanical strength, and resilience at elevated temperatures. Mullite is formulated to produce den.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Gouda Vuurvast ADHESIET 150 Dry Air-Setting Refractory Mortar Description: Adhesiet 150 is an air setting mortar with a sodium silicate bond and is supplied as a dry powder. Because of the special mix of the raw materials it can be used up to 1500°C.Remarks.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Gouda Vuurvast ADHESIET 170 P Al Dry Air-Setting Refractory Mortar Description: Adhesiet 170 P Al is a phosphate bonded air setting mortar, supplied as a dry powder. Because of the special choice of raw materials this mortar is especially applied in aluminum meltin.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Gouda Vuurvast AK 46 S Dense Refractory Brick Description: AK 46 S is a very dense, high quality firebrick with low iron and alkali content, characterized by a low creep (after 24 hours at 1280°C at a load of 0.2 MPa, the creep is only 0.05%.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Gouda Vuurvast AK 50 Dense Refractory Brick Description: This brick has a low iron and alkali content and is therefore suitable for use in reducing atmospheres at high temperatures. Very good resistance to slag attack. Application: incinerato.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Gouda Vuurvast CURAS SiC 90 D Moldable Refractory Material Description: This material is supplied as a dry powder. It has to be mixed with clean water to the necessary consistency. Curas SiC 90 has a phosphate bond and especially meant for protection of bo.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Misumi Alumina 99 Aluminum Oxide, Al2O3 Information provided by MISUMI Corporation. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Gouda Vuurvast AK 70 A Dense Refractory Brick Description: This brick is made of a high quality bauxite. Application: transition zone of rotary cement kiln.Remarks: This data represents average values, obtained from samples that were cut from s.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 70 A Dense Refractory Brick Description: This brick is made of a high quality bauxite. Application: transition zone of rotary cement kiln.Remarks: This data represents average values, obtained from samples that were cut from s.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Gouda Vuurvast CURON 150 HR GM Dense Refractory Castable Description: Curon 150 HR GM is a gunning castable, because of its low iron content also very well suitable under reducing circumstances. In addition, this castable has a good thermal shock resistan.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Gouda Vuurvast VIBRON 155 Dense Vibrating Refractory Castable Description: Vibron 155 is a vibrating castable based on sintered bauxite especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provid.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Sharadaa Ceramics HF 60 AL Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Sharadaa Ceramics Smart Cast 9 Medium Cement Castables Information provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Sapco 95% Aluminum Oxide Information provided by Sapco. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Sharadaa Ceramics VELCRETE G 401 Gunning Castables Description: Available from us a range of Gunning Castables that are made in compliance with the set industrial standards. These castables are widely used in refineries, foundries, boilers, rolling .. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Sharadaa Ceramics ZAP 011 Smart Cast Application Special Properties: Thermal Shock, Accretion, Co, Impact ResistanceIndustry: Sponge IronApplication: Sponge Rotary KilnInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
CeramTec 771 94% Alumina (Al2O3) Te value is 840°C. Hasselman Thermal Shock value is 200 K.Data provided by CeramTec North America. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
CeramTec RK 87 Alumina, 99.8% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
CeramTec Rocar® S Silicon Carbide, SSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | Continuous |
Zircar Ceramics ZAL-15AA Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | No Load |
CoorsTek AD-90 Alumina (nom. 90% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | NO-LOAD COND. |
CoorsTek DuraSense™ Ceramic Alumina Toughened Zirconia Oxygen ionic conductor for extreme-stress and extreme-thermal-shock environments |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | No Load |
CoorsTek Yttria Partially Stabilized Zirconia, YZTP, Sintered Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | No Load |
CoorsTek Zirconia-Toughened Alumina, ZTA Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Chosun Refractories 1500 ACE BLANKET Blanket Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Chosun Refractories 1500 ACE PAPER Paper Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | >= 1500 °C | >= 2730 °F | |
China-Yixing Longly Refractories 95 Alumina Ceramic Tubes & Rods LONGLY's alumina ceramic tubes and rods (the tolerances of +/- 0.02mm could be reached by mechanical or electronic finishing or mirror surface finishing) have high hardness, wear resistance, insulat.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2 950 has a combination of high strength (from zirconia) and high hardness (from the alumina phase). It has excellent wear resistance, both in sliding and abrasive conditions. This material offers a g.. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
CeramTec AT 79 Alumina, 99.6% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Maximum Service Temperature, Air | 1500 °C | 2730 °F | |
Gouda Vuurvast AK 50 A Dense Refractory Brick Description: This brick has a low porosity and a high strength and therefore a very good slag resistance. Applications: rotary cement kilns.Remarks: This data represents average values, obtained fro.. |