Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 66.7 °C | 152 °F | |
Bostik 130 General Purpose EVA Glue Stick Bostik 130 General Purpose EVA Glue StickGeneral purpose for a variety of substrates including ABS in general assembly. |