Polymer Property : Maximum Service Temperature, Air = 1600 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1300 - 1600 °C
2370 - 2910 °F
CeramTec SL200B Silicon Nitride
SL200B ceramic material was designed especially for use in the field of welding technology. SL200B is a 100 bar gas-pressure sintered silicon nitride (Si3N4) with impressive properties. It boasts de..