Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1610 °C
2930 °F
Anderman Ceramics EC100P Recrystallized Silicon Carbide
EC100P is a porous silicon carbide with excellent thermal shock resistance and high strength and high temperature operating capabilities up to 2910 °F (1600 °C). It is excellent for use in furnace..