Polymer Property : Maximum Service Temperature, Air = 163 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 73.0 °C
163 °F
Deflection temperature; load unknown.
Abatron AboCast 8-3/Abocure 8-3 Epoxy
2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 100 g (3.5 oz.): 265 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F)..