Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1000 °C @Pressure 6.89 MPa |
1832 °F @Pressure 1000 psi |
Continuous |
Garlock THERMA-PURâ„¢ 4122-CMG High Temperature Gasketing Material THERMa-PURâ„¢ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a u.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1832 °F | Continuous |
Garlock THERMA-PURâ„¢ 4122-KAMM High Temperature Gasketing Material THERMa-PURâ„¢ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a u.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1832 °F | |
Stellar Canada CERAMITE® CSR-F Wear Resistant Castable Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1832 °F | |
Stellar Canada CERAMITE® CSR-S Wear Resistant Castable Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w.. |
|||
Maximum Service Temperature, Air | 1000 °C | 1832 °F | No Load |
Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC Recommended for temperatures to 1472°F (800°C) and peaks up to 1832°F (1000°C). Demonstrates low thermal conductivity, high strength, high electrical insulation, zero porosity, non-wetting, and .. |
|||
Maximum Service Temperature, Air | 1000 °C @Pressure 3.45 MPa |
1832 °F @Pressure 500 psi |
Continuous |
Garlock THERMA-PUR™ 4122-FC High Temperature Gasketing Material THERMa-PUR™ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a uniqu.. |