Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1900 °C | 3450 °F | |
Gouda Vuurvast AC 90-8 Dense Refractory Brick Description: Excellent resistance against alkali- and metal slags. The 8% chromium-oxide addition gives good volume stability at very high temperatures. Applications: chemical incinerators, combusti.. |
|||
Maximum Service Temperature, Air | 1900 °C | 3450 °F | |
Zircar Refractory Composites RS-ZIRGUARD ZIRCONIA COATING ZRCI Zirconium Oxide Coating Type RS-ZIRGUARD is a cream colored, water based paint of Zirconium Oxide (ZrO2). It is produced using high-purity, partially stabilized Zirconium Oxide (4 wt% CaO). It .. |
|||
Maximum Service Temperature, Air | 1900 °C | 3450 °F | |
Anderman Ceramics EA999 Sintered Alumina, 99.9% Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |
|||
Maximum Service Temperature, Air | 1900 °C | 3450 °F | |
Anderman Ceramics EREC99 Cerium Oxide Rare earth refractory oxide ceramics exhibit very high thermal stability, wear resistance, and strength. They are widely used in applications above 3090 °F (1700 °C), nuclear, high performance met.. |