Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 89.0 °C | 192 °F | Heat deflection temperature, load unknown; ASTM D648 |
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Maximum Service Temperature, Air | 89.0 °C | 192 °F | Heat Distortion Temp |
Asahi Kasei Delpet® 60N Acrylic Molding Compound 60N is a medium grade of heat resistance and mechanical strength, allowing injection molding through relatively small gates and runners. General Delpet® qualities include attractive transparency, .. |
|||
Maximum Service Temperature, Air | 89.0 °C | 192 °F | Deflection Temp; Load not reported; ASTM D648 |
Asahi Kasei Delpet® 60N Acrylic Molding Compound 60N is a medium grade of heat resistance and mechanical strength, allowing injection molding through relatively small gates and runners. General Delpet® qualities include attractive transparency, .. |