Polymer Property : Maximum Service Temperature, Air = 2012.9 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1100.5 °C
2012.9 °F
Pyrotek S-1100 Compressible Insulation Board
The Pyrotek S-1100 board is a low density calcium silicate product typically used for back-up insulation in refractory constructions.ApplicationsReduction cell insulation Trough covers Back-up insul..