Maximum Service Temperature, Air 96.7 °C
206 °F
Heat Distortion, Annealed; ASTM D648
Total PSC 524B Polystyrene
Polystyrene 524B is a general purpose crystal polystyrene targeted for gloss coextrusion cap applications. It is specially formulated to reduce die buildup and die lines.Information provided by Tota..
Maximum Service Temperature, Air 96.7 °C
206 °F
Heat Distortion, Annealed; ASTM D648
Total PSC 525 Polystyrene
Polystyrene 525 is a crystal polystyrene for both injection molding and cap layer co-extrusion. Injection molding applications such as medical and laboratory parts, tumblers and jewel boxes demonstr..