Polymer Property : Maximum Service Temperature, Air = 217 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 103 °C
217 °F
Deflection Temp.; ASTM D648
NCMT NanoPAC™ HG500 High Performance Polypropylene Nanocomposite
Applications: Household Industry Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited
Maximum Service Temperature, Air 103 - 108 °C
217 - 226 °F
Softening Range
Huntsman AroCy M-10 Monomeric Bisphenol F Dicyanate
Comments/Applications: Very hydrophobic after cure. Monomeric tetramethyl bisphenol F dicyanate. Low viscosity impregnations.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has b..