Thermal Properties Metric English Comments
Maximum Service Temperature, Air 224 °C
435 °F
Master Bond EP30-3 High Temperature Resistant Two Component Epoxy
Master Bond Polymer System EP30-3 is a two component, low viscosity epoxy featuring optical clarity and high temperature serviceability up to 450°F along with superior chemical resistance. EP30-3 h..
Maximum Service Temperature, Air 224 °C
435 °F
Heat resistance per ASTM D794
Plenco 50335 PET, Pellet, Injection Molded, White  (discontinued **)
PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Inform..