Polymer Property : Maximum Service Temperature, Air = 23.9 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 23.9 °C
75.0 °F
Spartech RJ80598 PVC and Alloy Products for Wire and Cable
Information provided by Spartech
Maximum Service Temperature, Air 23.9 °C
75.0 °F
Spartech RJ8955FR-NAT PVC and Alloy Products for Wire and Cable
Information provided by Spartech
Maximum Service Temperature, Air 23.9 °C
75.0 °F
Spartech WJ8327CC PVC and Alloy Products for Wire and Cable
Information provided by Spartech