Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1270 °C | 2320 °F | |
Gouda Vuurvast CURON 127 S Dense Refractory Castable Description: Curon 127 S castable is characterized by a very high strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks: These value.. |
|||
Maximum Service Temperature, Air | 1270 °C | 2320 °F | |