Thermal Properties Metric English Comments
Maximum Service Temperature, Air 123 °C
253 °F
for 50% loss of tensile strength after 5000hr
BASF Ultramid® C3U BK 23079 PA6/66 FR (Conditioned)
Description: Injection-molding grade with improved flame retardance (free from halogens and phosphorus), used e.g. for impact resistant electrically insulating parts such as contact bases and plug c..
Maximum Service Temperature, Air 123 °C
253 °F
for 50% loss of tensile strength after 5,000 hr
BASF Ultramid® C3U PA66/6 (Conditioned)
Ultramid C3U is an injection molding, general purpose PA66/6 grade with improved flame retardance.
Maximum Service Temperature, Air 123 °C
253 °F
Deflection temperature; load unknown.
Abatron AboCast 50-11/AboCure 50-17 Epoxy
Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/27 ratio. Pot life: 500 g, 29 min. at 70°C (160°F). Exothermic Peak 270°C (520°F). Cures in 1-2 hrs at ..
Maximum Service Temperature, Air 123 °C
253 °F
Deflection Temp at unknown load
Abatron AboCast 8103-25 High-Performance Dielectric Epoxy
AboCast 8103-25 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system combines o..
Maximum Service Temperature, Air 123 °C
253 °F
for 50% loss of tensile strength after 5,000 hr
BASF Ultramid® C3U PA66/6 (Dry)
Ultramid C3U is an injection molding, general purpose PA66/6 grade with improved flame retardance.