Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 255 °C | 491 °F | |
Lehmann & Voss LUVOCOM® 1114-8364 PAEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Electrically conduct.. |
|||
Maximum Service Temperature, Air | 255 °C | 491 °F | |
Lehmann & Voss LUVOCOM® 1104-8327 Polyether ketone, with glass fiber, easy flowing Applications: Automotive industry, mechanical- and precision engineering.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts.Low warpage.Information pro.. |
|||
Maximum Service Temperature, Air | 255 °C | 491 °F | |
Lehmann & Voss LUVOCOM® 1114-0717 PAEK, with carbon fiber and PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Electrically conduct.. |
|||
Maximum Service Temperature, Air | 255 °C | 491 °F | Deflection Temp at unknown load |
Abatron AboCast 8501-6 One-Component Epoxy AboCast 8501-6 is a clear, high-temperature one-component epoxy system for very high-temperature uses. It offers the highest heat resistance of the clear resins. Suggested Uses: Casting; Potting; E.. |