Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1520 °C | 2770 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 44 Dense Refractory Brick Description: A very dense, high duty fireclay brick with low iron and alkali content. Widely used in anode-baking furnaces (aluminum industry) and as the lining of the top of blast furnaces.Remarks:.. |
|||
Maximum Service Temperature, Air | 1520 °C | 2770 °F | |
Sharadaa Ceramics HA 62 High Alumina Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1520 °C | 2770 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AK 50 A Dense Refractory Brick Description: This brick has a low porosity and a high strength and therefore a very good slag resistance. Applications: rotary cement kilns.Remarks: This data represents average values, obtained fro.. |