Thermal Properties Metric English Comments
Maximum Service Temperature, Air 287.8 °C
550.0 °F
Intermittent
Trelleborg Sealing Solutions HiMod® 914 Thermoplastic Bearing
Thermoplastic BearingCharacteristics: HiMod® 914 is a self lubricating bearing material developed for the most severe and critical applications. A high LPV along with good chemical resistance, low..
Maximum Service Temperature, Air 287.8 °C
550.0 °F
Intermittent
Trelleborg Sealing Solutions HiMod® 924 Thermoplastic Bearing
Thermoplastic BearingCharacteristics: HiMod® 924 is a high temperature, high modulus material developed for those functions that require high strength and high compressive properties along with exc..