Polymer Property : Maximum Service Temperature, Air = 3360 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1850 °C
3360 °F
Gouda Vuurvast CURAS 90 PF Moldable Refractory Material
Description: Curas 90 PF ramming mix with outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). The product is supplied in two components: a dry powder and a liquid. Curas 90 PF i..
Maximum Service Temperature, Air 1850 °C
3360 °F
Gouda Vuurvast CURAS 90 PF REPAIR Moldable Refractory Material
Description: Curas 90 PF Repair ramming mix is especially developed for repairing purposes of Curas 90 PF linings. The product is supplied in two components: a dry powder and a liquid. Detailed inst..
Maximum Service Temperature, Air 1850 °C
3360 °F
Gouda Vuurvast CURAS 90 PFM Moldable Refractory Material
Description: Curas 90 PFM ramming mix has outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). In addition, it has a good resistance against thermal shock and corrosive gasses. T..
Maximum Service Temperature, Air 1850 °C
3360 °F
Sharadaa Ceramics REFCAST HA PLUS High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Maximum Service Temperature, Air 1850 °C
3360 °F
Gouda Vuurvast LP 97-3 Dense Refractory Brick
Description: A high alumina quality brick containing a limited percentage of chromium oxide for improved slag resistance. The product has a very low silica- and iron oxide percentage so that it can ..