Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 183 - 207 °C | 361 - 405 °F | Average value: 196 °C Grade Count:10 |
Overview of materials for Phenolic, Resole, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Wood Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Maximum Service Temperature, Air | 183 °C | 361 °F | Heat Resistance; ASTM D570D |
Plenco 2369 Phenolic, Granular, Transfer Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |
|||
Maximum Service Temperature, Air | 183 °C | 361 °F | Heat Resistance; ASTM D570D |
Plenco 7100 Phenolic, Nodular, Injection Molded PLENCO 07100 is an organic fiber reinforced phenolic molding compound, with improved mechanical strength properties and an industrial finish. 07100 is densified for easy handling and good pourabilit.. |