Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 218 °C | 424 °F | Heat Resistance; ASTM D570D |
Plenco 08133 Polyester BMC, Compression Molded PLENCO 08133 is a renumber of PlasGlas 10313. PLENCO 08133 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co.. |
|||
Maximum Service Temperature, Air | 218 °C | 424 °F | Heat Resistance; ASTM D570D |
Plenco 1508 Polyester, Briquette, Injection Molded PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl.. |
|||
Maximum Service Temperature, Air | 218 °C | 424 °F | |
3M 33806 Premium Performance Aluminum Foil Tape High temperature acrylic adhesive of 425°FInformation provided by 3M |
|||
Maximum Service Temperature, Air | 218 °C | 424 °F | |
Hexcel® HexTOOL™ M61 Quasi-isotropic High Temperature Prepreg Tooling Compound HexTOOL™ Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequentl.. |
|||
Maximum Service Temperature, Air | 218 °C | 424 °F | |
3M 33801 Premium Performance Aluminum Foil Tape High temperature acrylic adhesive of 425°F. UL 723 ClassifiedInformation provided by 3M |
|||
Maximum Service Temperature, Air | 218 °C | 424 °F | Continuous |
Pyrotek AF-42 Spacer Bar Cover Long service life and excellent fit have made Pyrotek's Spacer Bar Covers a highly demanded product by leaders in the extrusion heat-treating industry. Manufactured from AF-42, a synthetic tex.. |