Polymer Property : Maximum Service Temperature, Air = 426 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 219 °C
426 °F
Heat resistance per ASTM D794
Plenco 6553 Phenolic, Granular, Compression Molded
Two-Stage Phenolic. PLENCO 06553 is a phenolic molding compound, formulated specifically for automotive brake pistons. 06553 exhibits excellent dimensional stability, and resistance to brake fluids..
Maximum Service Temperature, Air 219 °C
426 °F
3M 9740 Double Coated Tape
3M™ Double Coated Tape 9740 is a 3.5 mil double coated tape utilizing a 0.5 mil (12 microns) polyester film coated on both sides with 1.5 mils (38 microns) of a high shear acrylic adhesive system. ..