Maximum Service Temperature, Air 150 - 219 °C
302 - 426 °F
Average value: 185 °C Grade Count:15
Overview of materials for Phenolic; Unreinforced; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of..