Polymer Property : Maximum Service Temperature, Air = 489 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 254 °C
489 °F
Nylene® PA6/6 Glass/Mineral Filled 7215 HS Nylon 6/6
15% Glass Reinforced/25% Mineral Filled.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.