Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 56.7 °C | 134 °F | Heat Deflection; ASTM D648 |
Protective Coating PC-Concrete™ Epoxy Concrete Anchoring and Repair System PC Concrete™ epoxy gel is an anchoring and concrete repair product. PC Concrete™ is formulated for anchoring threaded rods, bolts, rebar dowels and smooth dowels into concrete, grout filled block,.. |