Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 327 °C | 621 °F | |
DuPont Performance Polymers Kalrez® 7075 FFKM Perfluoroelastomer Kalrez® Spectrum™ 7075 is designed specifically for the needs of the chemical processing industry. Compound 7075 broadens the family of Spectrum™ sealing options with a compound that has enhanced.. |