Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 350 °C | 662 °F | Maximum Operating Temperature |
Piezo Kinetics PKI 100 Lead Metaniobate Piezoelectric Lead Metaniobate exhibits properties not usually present in other types of piezoelectric ceramics. The noteworthy facts are its low mechanical QM, negligible aging, wide range of operating temperat.. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | |
Resinlab® RC8041 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | |
Resinlab® TL5022 Anaerobic Threadlocking Compound The TL5000 Series anaerobic threadlocking compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. They form a .. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | Reasonable mechanical properties retained |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of rod; more specific form/thickness entries are also available in MatWeb.Industry Specifications: USA Aeros.. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | Reasonable mechanical properties retained |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | Reasonable mechanical properties retained |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | Reasonable mechanical properties retained |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, 4.00-6.00 in, Annealed, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, 4.00-6.00 in, Annealed, Per Mil-T-9047G; other specific form/thickness entries .. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | Reasonable mechanical properties retained |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), >0.500-1.000 in, STD, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to >0.500-1.000 in, STD, Per Mil-T-9047G; other specific form/thickness entries are also available i.. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | Reasonable mechanical properties retained |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Rod, Square, or Hex, >2.000-3.000 in, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod, Square, or Hex, >2.000-3.000 in, Per Mil-T-9047G; other specific form/thickness entries are .. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | Reasonable mechanical properties retained |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; Medium To High Strength General-Purpose Alloy Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A .. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | Reasonable mechanical properties retained |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 2.50 - 4.00 in Rod or Thickness; Per ASTM F136) Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | |
Loctite® 5920™ RTV Silicone Sealant LOCTITE® 5920™ is a moisture-curing, non-corrosive silicone. The thixotropic nature of LOCTITE® 5920™ reduces the migration of liquid product after application to the substrate. It has been desi.. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | |
DuPont™ Kevlar® Aramid Pulp Sold as highly fibrillated, short (0.5-1mm) fibers. Kevlar® pulps are chopped fibers that can be used as specialty additives to enhance performance by providing excellent reinforcement and viscos.. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | Intermittent |
Epoxy Technology EPO-TEK® 383ND High Temperature Epoxy Material Description: A slightly longer pot life version of EPO-TEK®353ND designed for high temperature, optical and structural applications inside the semiconductor, hybrid, electronic, fiber opti.. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | Intermittent |
Epoxy Technology EPO-TEK® 430 Epoxy Product Description: A two component, copper-filled, electrically and thermally conductive epoxy for adhesive bonding in electronics. It may be used at the PCB level for interconnecting, grounding .. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | Intermittent |
Epoxy Technology EPO-TEK® H24 Electrically Conductive Epoxy Product Description: EPO-TEK® H24 is a two component, electrically and thermally conductive epoxy adhesive designed for semiconductor die attach and hybrid micro-electronics assembly.Advantages & A.. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | |
BASF Heligoen® Blue L 6875 H Color Additive Description: Reddish a-phthalocyanine blue with excellent flocculation resistance and dispersibility.Chemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: PowderSuitable for: Baking system.. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | |
BASF Heligoen® Blue L 7072 D Color Additive Description: ß-phthalocyanine blue with excellent dispersibilityChemical Structure: Cu-phthalocyanine, betaPhysical form: PowderSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate s.. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | |
Alliance C-5 Strontium Ferrite Ceramic Magnetic Material |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | |
Alliance C-8 Strontium Ferrite Ceramic Magnetic Material |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | |
Alliance C-8H Strontium Ferrite Ceramic Magnetic Material |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | |
Alliance C-9B Strontium Ferrite Ceramic Magnetic Material |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | |
BASF Heligoen® Green L 8731 Color Additive Description: Brilliant phthalocyanine greens, somewhat yellower than L 8690(L 8731 is especially for powder coatings)Chemical Structure: Cu-phthalocyanine, chlorinatePhysical form: PowderSuitable fo.. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | |
BASF Paliogen® Red L 3910 HD Color Additive Description: Perylene reds for shades with high brilliancy and opacitySuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing systems, Amine curing systems and Aird.. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | peak |
3M Dyneon™ 301Z Translucent Perfluoroelastomer System Features and Benefits:Excellent plasma resistance with low particle count Low extractables, low outgassing, and low particle generation for ultra high purity applicationsPhosphorous-free and silica.. |
|||
Maximum Service Temperature, Air | 350 °C | 662 °F | |
Resinlab® TL5090 Anaerobic Threadlocking Compound The TL5000 Series anaerobic threadlocking compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. They form a .. |