Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 68.3 °C | 155 °F | |
Spartech Polycast Solarcryl (0.187") Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Maximum Service Temperature, Air | 68.3 °C | 155 °F | |
Bostik 140 Low Cost EVA Glue Stick Bostik 140 Low Cost EVA Glue StickLow cost. General purpose for most porous substrates used for craft / floral applications. |