Polymer Property : Maximum Service Temperature, Air = 68.9 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 68.9 °C
156 °F
Bostik 2106 Low viscosity, quick grab EVA Glue Stick
Bostik 2106 Low viscosity, quick grab EVA Glue StickLow viscosity. Quick grab for woodworking, general assembly and various plastics.
Maximum Service Temperature, Air 68.9 °C
156 °F
Bostik 2103 Flexible Bond EVA Glue Stick
Bostik 2103 Flexible Bond EVA Glue StickFlexible bond for non-porous substrates.
Maximum Service Temperature, Air 68.9 °C
156 °F
Bostik 2128 Clear, Light Assembly EVA Glue Stick
Bostik 2128 Clear, Light Assembly EVA Glue StickClear for light assembly.
Maximum Service Temperature, Air 68.9 °C
156 °F
Bostik 2102 Fast Setting EVA Glue Stick
Bostik 2102 Fast Setting EVA Glue StickFast setting for packaging applications.