Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 870 °C | 1600 °F | Continuous |
Mykroy/Mycalex MM 800 Machining Grade Glass-bonded Mica Composite MM 800 (formerly MM 1600) is a compression molded glass mica composite that is the perfect alternative to high performance plastics where high temperature, good dielectric strength and good arc resi.. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | |
Pyrotek PROSILY G-10R Graphite Lubricant/Coating Color - Black, Base - Graphite, Carrier - ResinApplicationsMold coating Extrusion die Dry film lubricator AdvantagesResistant to high temperature Good thermal conductivity Low coefficient of expansi.. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | |
Pyrotek PROSILY G-11R Graphite Lubricant/Coating Color - Black, Base - Graphite, Carrier - ResinApplicationsMold coating Extrusion die Dry film lubricator AdvantagesResistant to high temperature Good thermal conductivity Low coefficient of expansi.. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | |
Pyrotek PROSILY G-40W Graphite Lubricant/Coating Color - Black, Base - Graphite, Carrier - WaterApplicationsStrip caster Roll lubricator AdvantagesResistant to high temperature Good thermal conductivity Low coefficient of expansion Chemically iner.. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | |
Pyrotek Stainless Steel Mesh Core Stainless steel mesh. Flat.AdvantagesExcellent Abrasion Resistance Good Compression and Recall Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | |
Pyrotek Steel Mesh Core Steel mesh. Tube shaped.AdvantagesExcellent Abrasion Resistance Good Compression and Recall Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | |
Gouda Vuurvast GOLITE 90 L Refractory Insulating Castable Description: Golite 90 L is a castable with an extremely low density, used at places where a very good insulation is required.Remarks: These values apply to cast products. Also available in gunning .. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | |
MetalTek MTEK 20-10 Cast UNS J92603 Heat Resistant Stainless Steel Economical heat resistant grade with sufficient chrome and nickel for good oxidation resistance.Applications: Burner tips, furnace rails, annealing boxes, trays, burnishing rolls.Information provide.. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | oxidation resistance, intermittent |
H.C. Starck Ampersint® AISI 316 L 300 µm For P/M, HIP/CIP, MIM AISI 316 L is a type of low carbon austenitic Cr-Ni-Mo stainless steel with good oxidation resistance in intermittent service to 870°C and in continuous service to 925°C, resistance to intercr.. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | oxidation resistance, intermittent |
H.C. Starck Amperweld® AISI 316 L 150/53 µm for Plasma Transferred Arc Surfacing AISI 316 L is a type of low carbon austenitic Cr-Ni-Mo stainless steel with good oxidation resistance in intermittent service to 870°C and in continuous service to 925°C, resistance to intercr.. |
|||
Maximum Service Temperature, Air | 870 °C | 1600 °F | oxidation resistance, intermittent |
H.C. Starck Ampersint® AISI 316 L 31 µm For P/M, HIP/CIP, MIM AISI 316 L is a type of low carbon austenitic Cr-Ni-Mo stainless steel with good oxidation resistance in intermittent service to 870°C and in continuous service to 925°C, resistance to intercr.. |