Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 91.1 °C | 196 °F | Heat Distortion, Annealed; ASTM D648 |
Total PSI 825 Polystyrene Polystyrene 825 is a high impact polystyrene for injection molding. They polymers ability to be molded on fast cycles with minimal stresses results in outstanding impact retention.Applications such .. |
|||
Maximum Service Temperature, Air | 91.1 °C | 196 °F | |
Bostik 1525 Medium Performance, Oil Resistant Polyamide Glue Stick Bostik 1525 Medium Performance, Oil Resistant Polyamide Glue StickMedium performance. Oil resistance for wood, fabric and other porous substrates primarily in woodworking assembly operation. |