Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 90.0 - 97.0 °C | 194 - 207 °F | Softening Range |
Huntsman Araldite GT 6063 Bisphenol A Epoxy Solid Resin Weight per Epoxide (EEW, g/eq) 640 to 730. Max color is 1.Comments/Applications: Unmodified bis A "Type 2 1/2" epoxy, non-sintering. Specifically designed for powder coatings, exceptional flow.Dat.. |
|||
Maximum Service Temperature, Air | 85.0 - 97.0 °C | 185 - 207 °F | Softening Range |