Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 97.2 °C | 207 °F | Heat Distortion, Annealed; ASTM D648 |
Total 680 Polystyrene
(discontinued **) Polystyrene 680 is a medium impact polystyrene developed for the foam extrusion and laminate markets. This polymers impact qualities in conjunction with its high flexural strength allow 680 to be ex.. |
|||
Maximum Service Temperature, Air | 97.2 °C | 207 °F | Heat Distortion, Annealed; ASTM D648 |
Total PSC 523 Polystyrene Polystyrene 523 is a high flow, high heat crystal. Specially designed for foam applications it has a very narrow molecular weight distribution. Performance in extruded loose fill foam is excellent d.. |