Polymer Property : Vicat Softening Point = 117 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 47.0 °C

@Load 5.10 kg
117 °F

@Load 11.2 lb
ISO 306
Borealis Borcom™ WE007AE Polypropylene
Borcom™ WE007AE is a polypropylene microcomposite intended for injection molding. The product is available in natural color. This material has an excellent balance between impact strength and stif..