Thermal Properties Metric English Comments
Vicat Softening Point 141 °C

@Load 1.00 kg
286 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPC K20040 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 141 °C

@Load 1.00 kg
286 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPHC K3020 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 141 °C

@Load 1.02 kg
286 °F

@Load 2.25 lb
ISO 306
Borealis Daplen™ EF267AI Polypropylene TPO Compound
Daplen™ EF267AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process...
Vicat Softening Point 141 °C

@Load 5.10 kg
286 °F

@Load 11.2 lb
50°C/h; ISO 306
Covestro Makrolon® Rx1851 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low..
Vicat Softening Point 141 °C

@Load 1.00 kg
286 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPHC K5020 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 141 °C

@Load 1.00 kg
286 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPHC K8020 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 141 °C

@Load 1.00 kg
286 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPHC K9020 Polypropylene, Mineral Reinforced