Thermal Properties Metric English Comments
Vicat Softening Point 147 °C

@Load 1.00 kg
297 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB SCANTEC PC S60R Polycarbonate
Information provided by Polykemi AB
Vicat Softening Point 147 °C

@Load 1.00 kg
297 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Wonderloy® PC-175D PC/ABS Alloy  (discontinued **)
Optical Disk
Vicat Softening Point 147 °C

@Load 1.02 kg
297 °F

@Load 2.25 lb
50°C per hour; ISO 306
Total PPH 7089 Polypropylene Homopolymer, Fiber
Polypropylene PPH 7089 is a narrow molecular weight distribution homopolymer polypropylene, with anti-gas fading stabilization.Polypropylene PPH 7089 is intended for the extrusion of fibers with the..
Vicat Softening Point 147 °C

@Load 1.02 kg
297 °F

@Load 2.25 lb
50°C per hour; ISO 306
Total PPC 3650 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 3650 is a heterophasic copolymer with a Melt Flow index of 2 g/10 min.Polypropylene PPC 3650 provides an excellent balance between toughness and flow, being particularly suitable i..
Vicat Softening Point 147 °C

@Load 5.00 kg
297 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTACARB 0820 GF V0 HF Flame Retardant Polycarbonate
Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, antimony, chlorine and bromine free, high stiffness, high dimensional stability, good processability, good light resistanceI..
Vicat Softening Point 147 °C

@Load 5.00 kg
297 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTACARB 0820 GF V0-5V Flame Retardant Polycarbonate
Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, PBDE free, high stiffness, high dimensional stability, good melt flow, good processability, good light resistanceInformation..
Vicat Softening Point 147 °C

@Load 5.00 kg
297 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTACARB 0820 GF V0-5V HF Flame Retardant Polycarbonate
Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, antimony, chlorine and bromine free, high stiffness, high dimensional stability, good melt flow rate, good processability, g..
Vicat Softening Point 147 °C

@Load 5.10 kg
297 °F

@Load 11.2 lb
50°C/h; ISO 306
Covestro Makrolon® 2400 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Vicat Softening Point 147 °C

@Load 5.10 kg
297 °F

@Load 11.2 lb
50°C/h; ISO 306
Covestro Makrolon® 2408 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Vicat Softening Point 147 °C

@Load 5.10 kg
297 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Makrolon® 2600 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Vicat Softening Point 147 °C

@Load 5.10 kg
297 °F

@Load 11.2 lb
50°C/h; ISO 306
Covestro Makrolon® 2800 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Vicat Softening Point 147 °C

@Load 5.10 kg
297 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Makrolon® 3107 MAS167 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig..
Vicat Softening Point 147 °C

@Load 5.10 kg
297 °F

@Load 11.2 lb
50°C/h; ISO 306
Covestro Makrolon® 3152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Vicat Softening Point 147 °C

@Load 5.10 kg
297 °F

@Load 11.2 lb
50°C/h; ISO 306
Covestro Makrolon® 3158 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Vicat Softening Point 147 °C

@Load 5.10 kg
297 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Makrolon® FU4007 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications..
Vicat Softening Point 147 °C

@Load 5.10 kg
297 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Makrolon® ET3227 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc..