Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 66.0 °C @Load 5.001 kg |
151 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP CIP6020F Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 66.0 °C @Load 5.10 kg |
151 °F @Load 11.2 lb |
ISO 306 |
Borealis ME268Al Polypropylene Compound, Mineral Filled ME268AI is a 20% mineral filled polypropylene compound intended for injection molding. Applications: ME268AI has been developed especially for the car industry to be used in automotive interior par.. |