Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 72.0 °C @Thickness 4.00 mm |
162 °F @Thickness 0.157 in |
Rate A; 10.0 mm wide molded rod; ISO 306/B50 |
Premix Thermoplastics PRE-ELEC® ESD 1100
(discontinued **) PRE-ELEC ESD 1100 is a static dissipative thermoplastic compound based on PETG. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 1100 has been developed for the e.. |
|||
Vicat Softening Point | 72.0 °C @Load 5.00 kg |
162 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
Chi Mei Kibiton® PB-5910 SBC High transparency, medium stiffness, toughness |
|||
Vicat Softening Point | 72.0 °C @Load 5.001 kg |
162 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC K9030 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |