Thermal Properties Metric English Comments
Vicat Softening Point 78.0 °C

@Load 5.10 kg
172 °F

@Load 11.2 lb
ISO 306
IPB Bicell® Cellular Polypropylene Sheet
Extruded, layered PP sheet, with a cellular core layer. Attributes include:Enhanced strength/thickness ratioOmni-directional flexural stresistanceHigh compression strengthWide variety of finishesRe..
Vicat Softening Point 78.0 °C

@Load 5.10 kg
172 °F

@Load 11.2 lb
50°C per hour; ISO 306
Total PPH 7089 Polypropylene Homopolymer, Fiber
Polypropylene PPH 7089 is a narrow molecular weight distribution homopolymer polypropylene, with anti-gas fading stabilization.Polypropylene PPH 7089 is intended for the extrusion of fibers with the..
Vicat Softening Point 78.0 °C

@Load 5.00 kg
172 °F

@Load 11.0 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-765 ABS - Flame Retardant
F.R. High Flow