Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 213 °C

@Load 1.00 kg
415 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB SCANMID 6 B12^ NH11L Nylon 6, Flame Retardant, Halogen Free
Information provided by Polykemi AB
Vicat Softening Point 213 °C

@Load 5.001 kg
415 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB SCANMID 6 B60 Nylon 6, Modified
Information provided by Polykemi AB