Polymer Property : Vicat Softening Point = 240 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 240 °C

@Load 5.00 kg
464 °F

@Load 11.0 lb
120°C/min; ASTM D1525/B, ISO 306/B
EPICHEM PA 66 GF 30 Polyamide 66, 30% Glass
Characteristics: 30% glass fibre filled
Vicat Softening Point 240 °C

@Load 0.999 kg
464 °F

@Load 2.20 lb
120°C/min; ASTM D1525/A, ISO 306/A
EPICHEM PA 66 Polyamide 66