Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 254 °C @Load 0.999 kg |
489 °F @Load 2.20 lb |
120°C/min; ASTM D1525/A, ISO 306/A |
EPICHEM Epinyl PA 66 GF 30 H Polyamide 66, 30% Glass, Heat Stabilized Characteristics: 30% glass fibre filled |
|||
Vicat Softening Point | 254 °C @Load 0.999 kg |
489 °F @Load 2.20 lb |
120°C/min; ASTM D1525/A, ISO 306/A |
EPICHEM Epinyl PA 66 GF 30 Polyamide 66, 30% Glass Characteristics: 30% glass fibre filled |