Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 160 °C @Load 1.00 kg |
320 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH DGF101015 PB Polypropylene Homopolymer, Glass Fibre/Mineral, Chemically Coupled Information provided by Polykemi AB |
|||
Vicat Softening Point | 160 °C @Load 1.00 kg |
320 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH GF15030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Vicat Softening Point | 160 °C @Load 1.00 kg |
320 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC GF3030 PD2 Polypropylene, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Vicat Softening Point | 160 °C @Load 5.001 kg |
320 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYform POM C M90 GF30 Polyoxymethylene Information provided by Polykemi AB |
|||
Vicat Softening Point | 160 °C @Load 5.10 kg |
320 °F @Load 11.2 lb |
50°C/hour; ISO 306 |
Ineos ABS Triax® 3158 ABS + Polyamide Blend (DAM), PA66/ABS Pellets (filled) Triax® 3158 is a PA+ABS-Blend and on-line paintable (195°C). It has very high heat resistance, reduced moisture, improved impact strength, and a low coefficient of linear thermal expansion. It.. |
|||
Vicat Softening Point | 160 °C @Load 5.10 kg |
320 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Styrolution Terblend® N 3158 ASA / PA, 9% Mineral filled Terblend® N 3158 is an 9% mineral-filled ABS/PA blend with good dimensional stability, enhanced rigidity and excellent heat resistance, so that this grade can be applied for online-painting.High .. |
|||
Vicat Softening Point | 160 °C @Load 1.02 kg |
320 °F @Load 2.25 lb |
ISO 306 |
Borealis GB205U Polypropylene Compound, Glass Fiber Reinforced GB205U is a 20% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Thi.. |
|||
Vicat Softening Point | 160 °C @Load 0.999 kg |
320 °F @Load 2.20 lb |
120°C/min; ASTM D1525/A, ISO 306/A |
EPICHEM Epilon PC GF 10 V0 Polycarbonate, 10% Glass Fiber Characteristics: self-extinguishing V0 at 1,6 mm, 10% glass fibre filled |