Vicat Softening Point 185 °C

@Load 1.00 kg
365 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB SCANLON A 5005 PA/ABS-Blend
Information provided by Polykemi AB
Vicat Softening Point 185 °C

@Load 1.00 kg
365 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB SCANLON A 5005B PA/ABS-Blend
Information provided by Polykemi AB
Vicat Softening Point 185 °C

@Load 1.00 kg
365 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB SCANLON A 5005B UV PA/ABS-Blend
Information provided by Polykemi AB
Vicat Softening Point 185 °C

@Load 0.999 kg
365 °F

@Load 2.20 lb
50°C/hr; ISO 306
Cossa Polimeri ESTABLEND PA 1424 GF HI ABS / Nylon 6 Blend, 12% Glass Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.12% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, high dimensional stabi..
Vicat Softening Point 185 °C

@Load 5.10 kg
365 °F

@Load 11.2 lb
cond.; ISO 306
Azoty Tarnow™ Tarnamid® T-27 MCS V0 Polyamide 6 - Flame Retarded, Unreinforced
Flame retarded (class V0), bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has th..
Vicat Softening Point 185 °C

@Load 5.10 kg
365 °F

@Load 11.2 lb
cond.; ISO 306
Azoty Tarnow™ Tarnamid® T-27 MCS V2 Polyamide 6 - Flame Retarded, Unreinforced
Flame retarded (class V2), bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has th..
Vicat Softening Point 185 °C

@Load 5.10 kg
365 °F

@Load 11.2 lb
cond.; ISO 306
Azoty Tarnow™ Tarnamid® T-27 MX6 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grade, reinforced with 10% hybrid mineral-glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good su..
Copyright © lookpolymers.com All Rights Reserved