Thermal Properties Metric English Comments
Vicat Softening Point 190 °C

@Load 1.00 kg
374 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYblend 6005 PC/ABS-Blend
Information provided by Polykemi AB
Vicat Softening Point 190 °C

@Load 1.00 kg
374 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYblend 6005B PC/ABS-Blend
Information provided by Polykemi AB
Vicat Softening Point 190 °C

@Load 1.00 kg
374 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYblend 6005B UV PC/ABS-Blend
Information provided by Polykemi AB
Vicat Softening Point 190 °C

@Load 0.999 kg
374 °F

@Load 2.20 lb
50°C/hr; ISO 306
Cossa Polimeri ESTABLEND PA 1050 GF HI ABS / Nylon 6 Blend, 25% Glass Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.25% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, high dimensional stabi..
Vicat Softening Point 190 °C

@Load 0.999 kg
374 °F

@Load 2.20 lb
50°C/hr; ISO 306
Cossa Polimeri ESTABLEND PA 2516 GF ABS / Nylon 6 Blend, 8% Glass Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.8% glass fiber reinforcedExceptional chemical resistance, excellent heat resistance, good dimensional stabilityInformation ..
Copyright © lookpolymers.com All Rights Reserved